Zhuang, Liwei, Peter Corkery, Dennis T. Lee, Seungjoon Lee, Mahdi Kooshkbaghi, Zhen-liang Xu, Gance Dai, IoannisG. Kevrekidis, and Michael Tsapatsis. 2021. “Numerical Simulation of Atomic Layer Deposition for Thin Deposit Formation in a Mesoporous Substrate”. AIChE J. 67. John Wiley & Sons, Inc.: e17305. Publisher’s Version: Numerical simulation of atomic layer deposition for thin deposit formation in a mesoporous substrate.